Description
Fractography of Glass, Softcover reprint of the original 1st ed. 1994
Coordinators: Bradt R.C., Tressler R.E.
Language: EnglishSubject for Fractography of Glass:
Publication date: 06-2013
302 p. · 15.5x23.5 cm · Paperback
302 p. · 15.5x23.5 cm · Paperback
Description
/li>Contents
/li>Comment
/li>
As the first major reference on glass fractography, contributors to this volume offer a comprehensive account of the fracture of glass as well as various fracture surface topography. Contributors discuss optical fibers, glass containers, and flatglass fractography. In addition, papers explore fracture origins; the growth of the original flaws of defects; and macroscopic fracture patterns from which fracture patterns evolve. This volume is complete with photographs and schematics.
Identation Fractography (B.R. Lawn, D.B. Marshall). Quantitative Fractographic Analysis of Fracture Origins in Glass (J.J. Mecholsky). Stress Wave Fractography (H. Richter, F. Kerkhof). Fractography of Stress Corrosion Cracking in Glass (T.A. Michalske). Fractography of Optical Fibers (H.C. Chandan et al.). Fractography of Fiberglass (P.K. Gupta). Fracture of Glass Containers (J.B. Kepple, J.S. Wasylyk). Fracture and Fractography of Flat Glass (N. Shinkai). Index.
This major reference on glass fractography offers a comprehensive account of the fracture of glass as well as various fracture surface topography. Contributors discuss optical fibers, glass containers, and flatglass fractography. In addition, papers explore fracture origins , the growth of the original flaws of defects , and macroscopic fracture patterns from which fracture patterns evolve.